公司新聞
瀝青料路面縱向接縫不良的問題預防
來源:http://guixin.net.cn/ 日期:2023-06-26
瀝青料路面接縫不良,會導致兩側(cè)標高不一,路面傾斜,在行車作用F,易發(fā)生顛簸或造成瀝青料松散。如伴隨壓實不足,在重交通作用下,易造成接縫處表層過度磨損,且不良的接縫易透水,水分經(jīng)接縫下滲,這會給路基、路面造成更大的破壞。
Poor joints in asphalt pavement can lead to uneven elevations on both sides, tilting of the road surface, and easy bumping or loosening of the asphalt material during driving. If accompanied by insufficient compaction, under the action of heavy traffic, it is easy to cause excessive wear on the surface of the joint, and poor joints are prone to water permeability. Water seeps through the joints, which will cause greater damage to the roadbed and road surface.
濟南瀝青料路面縱向接縫不良,易導致新舊攤鋪車道標高不易或接縫處混合料松散。
Poor longitudinal joints in Jinan asphalt pavement can easily lead to poor elevation of new and old paving lanes or loose mixture at the joints.
1、造成縱縫不良的基本原因
1. The basic reasons for poor longitudinal joints
(1)冷接縫施T工藝不規(guī)范:半幅施工不能采用熱接縫時易架設擋板或采用切片切齊。鋪另半幅前必須將縫邊緣清掃干凈,并涂抹少量粘層瀝青。攤鋪時應重疊在鋪層上5~lOcm,攤鋪后用人下將攤鋪在前半幅上面的混合料鏟走,然后再進行碾壓,應注意新攤鋪帶必須和前一條攤鋪帶松鋪厚度相同;否則,易造成新舊攤鋪車道不正確的重疊,重疊太多發(fā)生隆起,重疊太少就會低于先攤鋪的面層的標高;
(1) The cold joint construction process is not standardized: when half width construction cannot use hot joints, it is easy to install baffles or use slicing to cut evenly. Before laying the other half, the edge of the joint must be cleaned and a small amount of adhesive layer asphalt must be applied. When paving, it should overlap the paving layer by 5-lOcm. After paving, the mixture spread on the first half of the road should be removed by a person, and then compacted. It should be noted that the new paving strip must have the same loose paving thickness as the previous one; Otherwise, it is easy to cause incorrect overlap between the new and old paving lanes. If there is too much overlap, it will cause uplift, and if there is too little overlap, it will be lower than the elevation of the first paving surface layer;
(2)熱接縫施T工藝不規(guī)范:熱接縫施丁一般是在使用兩臺以上攤鋪機前后錯開10—20米成梯隊作業(yè)。此時兩條比鄰攤鋪帶的混合料還處于樂實前的熱狀態(tài),所以縱向接縫易于處理,且連接強度較好。施LT時應將以攤鋪的混合料部分留下10~20cm寬,暫不碾壓,作為后攤鋪部分的高層基準面,待后攤鋪部分完成后。一起碾壓(跨縫碾壓);否則壓實設備在接縫冷的一側(cè)壓槎太多,或是碾壓時瀝青混合料溫度不夠,這造成接縫處碾壓不實;
(2) The hot joint construction process is not standardized: Hot joint construction is generally carried out in a staggered manner of 10-20 meters before and after using two or more pavers. At this point, the mixture of the two adjacent paving belts is still in the hot state before Le Shi, so the longitudinal joint is easy to handle and the connection strength is good. When applying LT, the mixture to be spread should be left with a width of 10-20cm and not compacted temporarily. It should be used as the high-level reference plane for the later spreading part, and after the latter spreading part is completed. Rolling together (cross joint rolling); Otherwise, the compaction equipment will press too many joints on the cold side of the joint, or the temperature of the asphalt mixture will not be enough during compaction, which will cause incomplete compaction at the joint;
(3)冷、熱接縫施-T項目部技術(shù)交底不或沒有針對性,施工人員技術(shù)不熟練,如耙平施工方式不對,造成縱縫不是隆起,就是溝槽或傾斜;此外,不良的縱縫的形成與攤鋪機機架人員的操作水平及攤鋪機工作性能有關,如進口非接觸式找平系統(tǒng)的攤鋪機比滑靴和走鋼絲繩的平整度要好,還與熨平板前方推帶的混合料重量的變化,進料器或或螺旋攤鋪器是否超載等有關。
(3) Cold and hot joint construction - The technical disclosure of the T project department is not comprehensive or targeted, and the construction personnel are not proficient in technology. If the raking construction method is not correct, the longitudinal joint is either raised, grooved or inclined; In addition, the formation of poor longitudinal joints is related to the operational level of the paver frame personnel and the working performance of the paver. For example, the flatness of the imported non-contact leveling system paver is better than that of the sliding shoe and steel wire rope, and it is also related to changes in the weight of the mixture pushed in front of the iron plate, whether the feeder or spiral paver is overloaded, and so on.
2、預防措施
2. Preventive measures
嚴禁使用不帶平衡梁或沒有聲納控制的攤鋪機攤鋪,必須使用性能良好進口攤鋪機攤鋪;嚴格控制底基層和基層標高、橫坡度、平整度等指標,其合格率不低于95%。
It is strictly prohibited to use pavers without balance beams or sonar control for paving, and imported pavers with good performance must be used for paving; Strictly control the elevation, cross slope, flatness and other indicators of the subbase and base layer, with a qualification rate of no less than 95%.
瀝青料路面縱向接縫不良的問題預防事項就講解到這里了,希望能夠給您好的幫助,更多事項就來我們網(wǎng)站http://guixin.net.cn咨詢!
That's all for the prevention of poor longitudinal joints in asphalt pavement. We hope it can be helpful to you. For more information, please visit our website http://guixin.net.cn consulting service